WinSperse 1010
WinSperse 1010 | |
Low-polarity hyperdispersant for ceramic inkjet | |
Chemical Composition | General application guidance |
Block copolymer with low-polarity | Use 6-15% on dry pigment weight. |
Chemo-physical Properties | Application tips |
Appearance: yellowish paste Active ingredient: 100% Amine value(mgKOH/g): 36-44 | Add dispersant to grinding mixture before adding pigment. |
Characteristics | Package |
Contain multi-amine anchoring group for better binding to pigment surfaces. Reduce pigment coagulation and sedimentation, increase storage stability. Improve system fluidity, color strength, and gloss. Narrow pigment size distribution to achieve easier filtration. | Drum: 25kg/drum |
Application scope | Storage |
Specially designed to disperse inorganic pigments in low polar inkjet printing inks for ceramic applications. | Store in cool and dry places,good for 2 year. After partial use, re-seal the container. |
上一条:WinSperse 1510 | 下一条:WinSperse4010 |